Research Article

Plasticity Improvement of Ball-Spun Magnesium Alloy Tube Based on Stress Triaxiality

Table 3

Process parameters.

Process parametersDifferent ball diameters R (mm)

Δt (mm)0.20.20.3
f/mm/r0.20.30.2
R (mm)2.5, 3.0, 3.5, 4.0, 4.5

Process parametersDifferent amounts of thinning Δt (mm)

f/mm/r0.20.30.2
R (mm)334.5
Δt (mm)0.1, 0.2, 0.3, 0.4, 0.5

Process parametersDifferent feed ratios f (mm)

R (mm)2.52.53
Δt (mm)0.20.30.2
f/mm/r0.1, 0.15, 0.2, 0.25, 0.3