Research Article

Formation and Properties of the Ta-Y2O3, Ta-ZrO2, and Ta-TaC Nanocomposites

Figure 8

Average grain size for the Ta-xY2O3, Ta-xZrO2, and Ta-xTaC bulk nanocomposites (xā€‰=ā€‰0, 5, 10, 20, and 40 wt.%); data measured using AFM (not all AFM images and grain size distributions have been shown in this paper).