Low-Cycle Fatigue Properties of the X70 High-Frequency Electric-Resistant Welded Pipes
Figure 5
Typical fractures at the crack initiation zone of (a–d) the pipe bodies and (e–h) weld joints (a, b, e, f) with and (c, d, g, h) without surface finishing.