Research Article
Microstructure and Density of Sintered ZnO Ceramics Prepared by Magnetic Pulsed Compaction
Figure 6
Perpendicular and parallel cross-sectional microstructures of the ZnO ceramics compacted by MPC and sintered at 1300°C for 2 h recorded from (a) central region and (b) outer region.
(a) |