Research Article
Influence of Processing Parameters on Laser Direct Joining of CFRTP and Stainless Steel
Figure 13
The morphology of debonding surface of the stainless steel/CFRTP joints with different clamping pressure after tensile: (a) 0.5 MPa, (b) 0.6 MPa, (c) 0.7 MPa, (d) 0.8 MPa, and (e) 0.9 MPa.
(a) |
(b) |
(c) |
(d) |
(e) |