Research Article
Change of Pore-Fracture Structure of Anthracite Modified by Electrochemical Treatment Using Micro-CT
Figure 8
Pore size distribution of samples with a diameter of 2.54 mm before and after modification. (a) Sample modified in the anodic zone; (b) sample modified in the cathodic zone.
(a) |