Linear correlation analyses between the proportion of nano-ZnO in MUF glues (x(ZnO)/(MUF)) and the selected properties of PBs containing nano-ZnO (y).

Properties of PBsnRR2TPy = a + b × x

Density (kg·m−3)30−0.030.00−0.160.88641.3 − 0.06 × /
Thickness swelling after 2 h (%)400.110.010.700.496.49 + 0.01 × /
Thickness swelling after 24 h (%)40−0.050.00−0.320.7518.12 − 0.01 × /
Water absorption after 2 h (%)40−0.150.02−0.920.3617.19 − 0.03 × /
Water absorption after 24 h (%)40−0.270.07−1.700.1045.47 − 0.14 × /
Internal bond strength (N·mm−2)50−0.390.16−3.030.000.40 − 0.004 × /
Bending strength (N·mm−2)30−0.130.02−0.790.439.03 − 0.02 × /