Sensitivity of Service Life Extension and CO2 Emission due to Repairs by Silane Treatment Applied on Concrete Structures under Time-Dependent Chloride Attack
Figure 1
Chloride profile: with and without silane treatment. (a) Chloride-depth profile. (b) Chloride-time profile.