Research Article
Porogenic Behavior of Water in High-Alumina Castable Structures
Figure 6
Effects of water content (W vol.%) on compositions’ apparent viscosity (η, mPa·s−1, measured at 50 s−1 and 25°C) and linear shrinkage after drying (LS, %, after 24 h at 120°C, for samples cured in the conventional static way).