Experimental results of energy dissipation.

SpecimenEnergy dissipation (kN·mm)Relative energy dissipation

RCB-06008.031.00
RCB-335877.430.98
RCB-666044.271.01
RCB-1003090.230.51
HRCB-05813.111.00
HRCB-335799.320.99
HRCB-664309.040.74
HRCB-1002995.920.52