Carbon Nanotube Fiber Pretreatments for Electrodeposition of Copper
Table 2
Used CNT fiber pretreatment methods.
| Treatment no. | Procedure |
| 1 | Heat treatment, 400°C, 10 min | 2 | Watts bath immersion, 72 h | 3 | Watts bath immersion, 60 min | 4 | Watts bath immersion, 30 min + rinsing | 5 | Boric acid immersion, 60 min | 6 | Anodization for 50 s, 2500 mV versus SCE |
|
|