Research Article
Experimental Investigation on the Behavior of Iron Powder-Reinforced Sand under Electromagnetic Field
| (kPa) | Sand (kPa) | Iron-powdered sand (kPa) | Iron-powdered sand under 0.5 A (kPa) | Iron-powdered sand under 1 A (kPa) | Iron-powdered sand under 2 A (kPa) |
| Relative density at 60% | 103 | 30409.68 | 16464.47 | 22983.93 | 31533.01 | 38477.60 | 206 | 42855.95 | 33820.75 | 42773.88 | 50010.53 | 56840.49 | 310 | 61040.02 | 55637.26 | 62280.16 | 65811.87 | 76135.43 |
| Relative density at 80% | 103 | 35069.21 | 33076.31 | 34522.15 | 37699.62 | 41039.19 | 206 | 48027.40 | 48448.40 | 54550.36 | 65218.19 | 68462.87 | 310 | 77618.35 | 80643.42 | 85292.63 | 66799.12 | 70504.34 |
|
|