Research Article
Experimental Investigation on the Behavior of Iron Powder-Reinforced Sand under Electromagnetic Field
| (kPa) | Sand (kPa) | Iron-powdered sand (kPa) | Iron-powdered sand under 0.5 A (kPa) | Iron-powdered sand under 1 A (kPa) | Iron-powdered sand under 2 A (kPa) |
| Relative density at 60% | 103 | 287.82 | 298.78 | 307.69 | 312.49 | 318.65 | 206 | 580.43 | 596.19 | 612.23 | 622.92 | 641.42 | 310 | 842.89 | 870.30 | 890.86 | 904.56 | 938.83 |
| Relative density at 80% | 103 | 306.25 | 344.63 | 364.64 | 370.05 | 377.42 | 206 | 627.93 | 673.69 | 692.13 | 746.95 | 774.36 | 310 | 871.28 | 952.53 | 986.80 | 1027.91 | 1041.62 |
|
|