Experimental Investigation on the Behavior of Iron Powder-Reinforced Sand under Electromagnetic Field
Table 4
Brittleness.
(kPa)
Sand (kPa)
Iron-powdered sand (kPa)
Iron-powdered sand under 0.5 A (kPa)
Iron-powdered sand under 1 A (kPa)
Iron-powdered sand under 2 A (kPa)
Relative density at 60%
103
0.09
0.07
0.11
0.13
0.14
206
0.09
0.08
0.08
0.09
0.08
310
0.09
0.07
0.07
0.07
0.11
Relative density at 80%
103
0.11
0.08
0.12
0.16
0.15
206
0.11
0.10
0.10
0.11
0.11
310
0.13
0.08
0.08
0.08
0.14
We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.