Research Article
Experimental Investigation on the Behavior of Iron Powder-Reinforced Sand under Electromagnetic Field
Table 5
Energy absorption capacity.
| (kPa) | Sand (kPa) | Iron-powdered sand (kPa) | Iron-powdered sand under 0.5 A (kPa) | Iron-powdered sand under 1 A (kPa) | Iron-powdered sand under 2 A (kPa) |
| Relative density at 60% | 103 | 3173.38 | 3253.88 | 3500.11 | 3518.13 | 3802.56 | 206 | 6355.85 | 6453.01 | 6432.52 | 6812.96 | 6773.75 | 310 | 8865.79 | 9128.71 | 9585.37 | 9443.23 | 9745.08 |
| Relative density at 80% | 103 | 3541.93 | 3554.64 | 3788.64 | 3864.91 | 3819.25 | 206 | 6349.85 | 7497.74 | 7359.33 | 7959.01 | 7762.73 | 310 | 9117.75 | 10255.34 | 10546.79 | 10721.98 | 10820.73 |
|
|