Investigation of Microstructural Damage in Ultrahigh-Performance Concrete under Freezing-Thawing Action
Figure 4
Cracked UHPC specimens (40 mm × 40 mm × 160 mm) after enduring 250 freezing-thawing cycles: (a) plain UHPC and (b) UHPC-1%.