Deposition of Coating to Protect Waste Water Reservoir in Acidic Solution by Arc Thermal Spray Process

Figure 6

Potentiodynamic plots of the SS plate and sprayed coatings in pH 4 solution after 312 h of exposure (1 mV/s).