Electrochemical parameters of the SS plate, SS-sprayed coating, and Ti-sprayed coating extracted after fitting of EIS data to suitable EECs with different exposure periods in pH 4 solution.

Time (h)1312

Sample IDSS plateSS sprayedTi sprayedSS plateSS sprayedTi sprayed
Rs (kΩ·cm2)6.775.208.645.025.378.45
Rp (kΩ·cm2)166.0016.0248.1922.8220.1521.07
CPE1
Q1 (1 × 10−6) (Ω−1·cm−2·sn)2.762.07.329.641.637.2
0.990.990.990.950.920.93
Ceff1 (µF·cm−2)2.6862.07.2229.041.036.5
Rct (kΩ·cm2)11.879.1510.97350.0211.5646.33
CPE2
Q2 (1 × 10−6) (Ω−1·cm−2·sn)91.6252.3105.820.9156.138.5
0.750.440.540.910.460.60
Ceff2 (µF·cm−2)94.19731.72120.1125.44312.1356.62
W (1 × 10−6) (Ω·cm2·s−0.5)4.2