Research Article
Degradation of Roller-Compacted Concrete Subjected to Freeze-Thaw Cycles and Immersion in Potassium Acetate Solution
Figure 4
Surface of the specimens subject to the F-T cycles in KAc solution: (a) 100; (b) 150; (c) 200; (d) 250.
(a) |
(b) |
(c) |
(d) |