Research Article
Mode-I Metal-Composite Interface Fracture Testing for Fibre Metal Laminates
Table 2
Adjusted normal interfacial strength with respect to different mesh sizes.
| Ne | le = 1 mm | le = 0.5 mm | le = 0.3 mm | (MPa) | (mm) | (MPa) | (mm) | (MPa) | (mm) |
| 1 | 25.5 | 1.0 | 36.1 | 0.5 | 45.8 | 0.3 | 3 | 14.7 | 3.0 | 20.8 | 1.5 | 26.4 | 0.9 | 5 | 11.4 | 5.0 | 16.1 | 2.5 | 20.5 | 1.5 | 8 | 9.0 | 8.0 | 12.8 | 4.0 | 16.2 | 2.4 |
|
|