Research Article

Effect of Copper and Iron Ions on the Sulphidizing Flotation of Copper Oxide in Copper Smelting Slag

Figure 3

Recovery of CuO under different conditions: (a) different pH values (Na2S 0.156 g/L); (b) different Na2S concentrations (pH = 10, neither CuSO4 nor Fe3Cl addition); (c) different CuSO4 concentrations (pH = 10, Na2S 0.156 g/L); (d) different Fe3Cl concentration (pH = 10, Na2S 0.156 g/L).
(a)
(b)
(c)
(d)