Research Article

Microstructure Evolution and Surface Cracking Behavior of Superheavy Forgings during Hot Forging

Figure 3

Microstructure of 18Mn18Cr0.6N steel compressed at 1150°C and 10−4·s−1 to different strains. (a) 0.2, (b) 0.4, (c) 0.6, and (d) 0.8.
(a)
(b)
(c)
(d)