Investigation on the Deterioration Mechanism of Recycled Plaster
Table 2
Properties of POP and R-P under the similar SSA.
| Gypsum | SSA (m2·kg−1) | W/P | Setting time (min) | 2 h strength (MPa) | Dry strength (MPa) | Water absorption (%) | Initial | Final | Flexural strength | Compressive strength | Flexural strength | Compressive strength |
| POP | 1098 | 0.68 | 26 | 30 | 2.47 | 4.59 | 4.50 | 6.98 | 38.89 | R-P | 1114 | 0.85 | 33 | 46 | 1.66 | 2.94 | 2.70 | 4.80 | 40.65 |
|
|