Research Article
Investigations on the Wear Rate of Sintering Diamond Core Bit during the Hole Drilling Process of Al2O3 Bulletproof Ceramics
| Test no. | Bit performance parameters | Number of water gaps | Wall thickness (mm) | Technological parameters | Number of machined holes | Grit size (mesh) | Concentration (%) | Bit load (N) | Spindle speed (rpm) |
| 1 | 35/40 | 75 | 3 | 2 | 352 | 3200 | 23 | 2 | 50/60 | 75 | 3 | 2 | 352 | 3200 | 13 | 3 | 35/40 | 125 | 3 | 2 | 352 | 3200 | 26 | 4 | 35/40 | 75 | 2 | 2.5 | 278 | 3200 | 33 | 5 | 35/40 | 75 | 4 | 2.5 | 278 | 3200 | 21 | 6 | 45/50 | 125 | 4 | 2 | 390 | 3200 | 15 | 7 | 45/50 | 125 | 4 | 2.5 | 390 | 3200 | 9 | 8 | 35/40 | 75 | 3 | 1.5 | 352 | 3200 | 9 | 9 | 45/50 | 125 | 4 | 2.5 | 278 | 3200 | 23 | 10 | 35/40 | 75 | 3 | 2 | 352 | 1750 | 21 |
|
|