Research Article
Self-Healing of Concrete Cracks by Ceramsite-Loaded Microorganisms
Table 2
Strength of mortar specimens containing ceramsite treated at different temperatures.
| Mechanical tests | Room temperature | 600°C | 750°C | 900°C |
| Compressive strength (MPa) | 36.39 | 33.42 | 35.58 | 35.68 | Flexural strength (MPa) | 8.10 | 8.32 | 7.77 | 8.48 |
|
|