Improvement for Construction of Concrete-Wall with Resistance to Gas-Explosion

Table 1

Experimental plan.

Mixing propertiesTest items

w/b0.50Fresh concreteSlump
Air content
Water content (kg/m3)220

S/a0.55Hardened concreteCompressive strength at 7 and 28 days
Flexural strength at 7 and 28 days
Tensile strength at 7 and 28 days
Impact of high-velocity projectile
Target slump (mm)150 ± 20
Target air content (%)4.5 ± 1.5
Binder composition (by weight)OPC : BS : FA = 7 : 2 : 1
Fiber content (%)1
Fiber combinationSF only
PF only
SF + PF