Figure 6

Drying shrinkage of paste specimens with binder types for (a) 180 days and (b) 14 days.
(a)
(b)

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.