Mix proportion of fiber concrete.
| Fiber | W/C (%) | s/a (%) | Volume fractions of fiber (%) | Unit content (kg/m3) | Additive (cc/m3) | Water | Cement | Sand | Gravel | Fly ash | Fiber | SP |
| PE | 45 | 47 | 0.25 | 175 | 389 | 618 | 879 | 137 | 2.43 | 0.97 | PVA | 0.19 |
|
|
SP, superplasticizer.
|