Research Article
Evaluation of Self-Healing Performance of PE and PVA Concrete Using Flexural Test
| Case | Days after casting | Healing | 1st and 2nd loading | 3rd loading | Condition | Period |
| PE-7–28-A PVA-7–28-A | 7 | 28 | Air | 21 days | PE-7–28-W PVA-7–28-W | Water |
| PE-28–49-A PVA-28–49-A | 28 | 49 | Air | 21 days | PE-28–49-W PVA-28–49-W | Water |
| PE-49–70-A PVA-49–70-A | 49 | 70 | Air | 21 days | PE-49–70-W PVA-49–70-W | Water |
| PE-91–112-A PVA-91–112-A | 91 | 112 | Air | 21 days | PE-91–112-W PVA-91–112-W | Water |
|
|