Review Article

A Review on Superplastic Formation Behavior of Al Alloys

Figure 2

ODFs representative sections of the Al-Zn-Mg-0.25Sc-0.10Zr alloy deformed at 500°C and 1 × 10−2·s−1 after interrupting the tensile test at different strains: (a) ε = 0; (b) ε = 0.69; (c) ε = 1.10; (d) ε = 2.40 [42].
(a)
(b)
(c)
(d)