Cross-sectional TEM image (a), EDS line profile (b), EDS quantitative analysis of selected points , , and (c), and SAEDs (d-e) of regions and in rust formed during 56-day immersion of 18Mn5Cr in 3.5% NaCl solution at 60°C, where subscript M indicates magnetite.
(a)
(b)
(c)
(d)
(e)