Research Article
Influences of Ultrafine Slag Slurry Prepared by Wet Ball Milling on the Properties of Concrete
Table 4
Designations of mixtures in this research.
| Number | GGBFS | Cement (wt.%) | Sand (wt.%) | Coarse (wt.%) | Water (wt.%) | Content (wt.%) | Milling duration (min) |
| A | A1 | 0 | ā | 100 | 157 | 236 | 50 |
| B | B1 | 20 | 0 | 80 | 157 | 236 | 50 | B2 | 35 | 0 | 65 | 157 | 236 | 50 | B3 | 50 | 0 | 50 | 157 | 236 | 50 |
| C | C1 | 20 | 20 | 80 | 157 | 236 | 50 | C2 | 35 | 20 | 65 | 157 | 236 | 50 | C3 | 50 | 20 | 50 | 157 | 236 | 50 |
| D | D1 | 20 | 40 | 80 | 157 | 236 | 50 | D2 | 35 | 40 | 65 | 157 | 236 | 50 | D3 | 50 | 40 | 50 | 157 | 236 | 50 |
| E | E1 | 20 | 60 | 80 | 157 | 236 | 50 | E2 | 35 | 60 | 65 | 157 | 236 | 50 | E3 | 50 | 60 | 50 | 157 | 236 | 50 |
|
|