Electrochemical Reduction of Industrial Baths Used for Electropolishing of Stainless Steel
Figure 4
Enhanced gloss after electropolishing in a bath without ER and with ER (EP process parameters: t = 45–180 min, I = 1.75 A, i = 0.05 A·cm−2, q = 2.25–9.00 Amin·cm−2, and T = 55°C).