Research Article
Electrochemical Reduction of Industrial Baths Used for Electropolishing of Stainless Steel
Figure 5
Topography of sample surface after electropolishing (parameters of the EP process: t = 180 min, i = 0.05 A·cm−2, q = 9.00 Amin·cm−2, and T = 55°C): (a) in a bath with ER and (b) in a bath without ER.
(a) |