Research Article
Influence of Rare Earth on Dynamic Recrystallization Behavior of As-Cast 30Mn Steel
Figure 5
Dynamic recrystallization volume fraction curves under various strain rates and a constant temperature (1050°C) of #1 and #2 samples. (a) = 0.1 s−1; (b) = 0.5 s−1; (c) = 1 s−1.
(a) |
(b) |
(c) |