Behavior of Chinese Dahurian Larch Wood after High-Temperature Exposure: Degradation of Mechanical Properties and Damage Constitutive Model
Table 1
Details of wood specimens for each test.
| Group | Notation | Number of specimens | Exposure temperature (°C) | Exposure time (min) | Cooling method |
| | W-R | 6 | 25 | — | — |
| Group A | W-T100E15NC | 6 | 100 | 15 | NC | W-T150E15NC | 6 | 150 | 15 | NC | W-T200E15NC | 6 | 200 | 15 | NC | W-T250E15NC | 6 | 250 | 15 | NC |
| Group B | W-T100E30NC | 6 | 100 | 30 | NC | W-T150E30NC | 6 | 150 | 30 | NC | W-T200E30NC | 6 | 200 | 30 | NC | W-T250E30NC | 6 | 250 | 30 | NC | W-T100E30WC | 6 | 100 | 30 | WC | W-T150E30WC | 6 | 150 | 30 | WC | W-T200E30WC | 6 | 200 | 30 | WC | W-T250E30WC | 6 | 250 | 30 | WC |
| Group C | W-T100E45NC | 6 | 100 | 45 | NC | W-T150E45NC | 6 | 150 | 45 | NC | W-T200E45NC | 6 | 200 | 45 | NC | W-T250E45NC | 6 | 250 | 45 | NC |
|
|
Note. NC, natural cooling; WC, water cooling.
|