Research Article

Sintering Behavior and Properties of Mo-Cu Composites

Figure 4

Fractograph of Mo-Cu compacts at different sintering temperatures: (a) 900°C, (b) 1000°C, (c) 1100°C, (d) 1200°C, and (e) 1300°C.