Research Article

Investigating the Material Removal Rate Parameters in ECM for Al 5086 Alloy-Reinforced Silicon Carbide/Flyash Hybrid Composites by Using Minitab-18

Table 5

SN response of machining.

LevelFVE

149.2348.5248.96
250.1148.2847.73
347.1148.5248.38
446.9848.1048.36
Delta3.130.431.23
Rank132