Research Article
Experience Study on Long-Life Microsurfacing with High Water Resistance Performance
Table 2
Technical specifications of modified emulsified asphalt.
| Test items | Test results | Technical indicators |
| Evaporation residual mass fraction/% | 63.6 | ≧60 | Remaining amount on the screen/% (1.18 mm screen) | 0.02 | ≦0.1 | Storage stability/1d | 0.8 | ≦1 | Enge La viscosity/E25 | 11.76 | 3–30 | Residual penetration/0.1 mm | 70.5 | 40–100 | Residual softening point/°C | 57 | ≧57 | Residual ductility | 26 | ≧30 |
|
|