Role of Glass Composition on Mechanical Properties of Shape Memory Alloy-Metallic Glass Composites

Figure 6

The atomic configurations of the monolithic MGs at the end stage of tensile loading. The strain value for Cu50Zr50, Cu54Zr46, Cu60Zr40, and Cu64Zr36 is 26.2%, 25.8%, 24.7%, and 24.8%, respectively.