Research Article
Fabrication, Characterization, and Impact of Heat Treatment on Sliding Wear Behaviour of Aluminium Metal Matrix Composites Reinforced with B4C
Figure 4
Microstructure examinations of pure Al7075, as-cast, and age-hardened specimens. (a) Al7075 alloy. (b) Al7075/B4C-6 wt.% as-cast. (c) Al7075/B4C-8 wt.% as-cast. (d) Al7075/B4C-10 wt.% as-cast. (e) Al7075/B4C-12 wt.% as-cast. (f) Al7075/B4C-6 wt.% age-hardened. (g) Al7075/B4C-8 wt.% age-hardened. (h) Al7075/B4C-10 wt.% age-hardened. (i) Al7075/B4C-12 wt.% age-hardened.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |
(i) |