Research Article
Constitutive Characteristics, Microstructure, and Texture Evolution of As-Cast 42CrMo Alloy in Nonisothermal Multipass Compression
Figure 3
True stress-strain curves of as-cast 42CrMo alloy at different finishing temperatures of (a) 990°C, (b) 1030°C, (c) 1070°C, and (d) peak stress of each pass during nonisothermal multipass compression.
(a) |
(b) |
(c) |
(d) |