| Specimen number | (KN) | | (KN) | |
| SFRP-1 | 457.0 | 0.0230 | 19846.86 | 0.93 | SFRP-2 | 434.0 | 0.0252 | 17209.04 | 0.81 | SFRP-3 | 432.0 | 0.0241 | 17908.36 | 0.84 | SFRP-4 | 408.4 | 0.0482 | 8465.018 | 0.40 | SFRP-5 | 269.1 | 0.0241 | 11155.42 | 0.52 | SFRP-6 | 326.0 | 0.0208 | 15648.00 | 0.73 | SFRP-7 | 318.0 | 0.0154 | 20715.43 | 0.97 | SFRP-8 | 467.1 | 0.0219 | 21299.31 | 1.00 | SFRP-9 | 341.0 | 0.0132 | 25916.00 | 1.22 | SFRP-10 | 384.7 | 0.0274 | 14033.86 | 0.66 | SFRP-11 | 392.2 | 0.0395 | 9935.73 | 0.47 |
|
|