Research Article
Effect of Cyclic Cryogenic Treatment on Wear Resistance, Impact Toughness, and Microstructure of 42CrMo Steel and Its Optimization
Figure 8
SEM micrographs of worn surfaces of (a) CHT specimens and CT specimens treated at (b) −120°C, (c) −160°C, and (d) −196°C.
(a) |
(b) |
(c) |
(d) |