Estimating the Asphalt Binder Film Thickness Using Scanning Electron Microscope and Energy Dispersive X-Ray Spectroscopy

Figure 9

SEM images of HMA at 150°C and optimized binder content of 4.23%: (a) asphalt mortar at magnification ×250 and bar scale 100 μm. (b) Asphalt mortar at magnification ×300 and bar scale 50 μm. (c) Filler particles at magnification × 5000 and bar scale 5 μm. (d) Asphalt binder film at magnification ×10,000 and bar scale 1 μm. (e) Asphalt binder film at magnification ×30,000 and bar scale 0.5 μm. (f) Elemental composition of asphalt binder film at point Y in image (e) by EDS.
(a)
(b)
(c)
(d)
(e)
(f)