Test ratios of phase 2.

Group numberCement content (%)WCP content (%)Water-reducing agent content (%)

WCP70WR0.02530700.025
WCP70WR0.0530700.05
WCP80WR0.0520800.05
WCP80WR0.120800.1
WCP90WR0.0510900.05
WCP90WR0.110900.1
WCP90WR0.1510900.15