Research Article

Effect of Dispersoids and Intermetallics on Hardening the Al-Si-Cu-Mg Cast Alloys

Figure 9

Variation in ∆P as a function of aging condition: (a) 155°C, (b) UTS-190°C, (c) YS-190°C, (d) % El-190°C, and (e) 350°C.
(a)
(b)
(c)
(d)
(e)