Normalized values for the output response.

Run orderMicrohardness (HV)Tensile strength (MPa)

11.0000.594
20.8950.583
30.7890.556
40.5090.488
50.5960.276
60.7190.918
70.0000.000
80.3861.000
90.2280.533