Grey relation analysis result.

GRC valuesGRGRank
Run orderMicrohardness (HV)Tensile strength (MPa)

11.0000.5520.7761
20.8260.5450.6864
30.7040.5300.6175
40.5040.4940.4996
50.5530.4080.4817
60.6400.8590.7502
70.3330.3330.3339
80.4491.0000.7243
90.3930.5170.4558