Research Article
Effect of Fiber Content on Mechanical Properties and Microstructural Characteristics of Alkali Resistant Glass Fiber Reinforced Concrete
Table 2
ARGFRC mixture proportion design.
| Component | FC0 | FC0.3 | FC0.5 | FC0.8 | FC1.0 | FC1.3 | FC1.5 |
| Cement (kg/m3) | 500 | 500 | 500 | 500 | 500 | 500 | 500 | Stone (kg/m3) | 1045 | 1045 | 1045 | 1045 | 1045 | 1045 | 1045 | River sand (kg/m3) | 700 | 700 | 700 | 700 | 700 | 700 | 700 | Water (kg/m3) | 200 | 200 | 200 | 200 | 200 | 200 | 200 | Water-reducing agent (kg/m3) | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 | Fiber volume content (m3) | 0.0% | 0.3% | 0.5% | 0.8% | 1.0% | 1.3% | 1.5% |
|
|
Note. FC-0.5 indicates 0.5% fiber content (by volume) of ARGFRC.
|